API 6A Bolting Torque for Flanges (SI Units)

This table gives the recommended make-up torque for API 6A flange bolting from API 6A (21st edition) Annex H, Table H.1 (SI units), for ASTM A453 Grade 660 Class D studs with Sy = 720 MPa tightened to a bolt stress of 360 MPa, half the yield strength. Torque applied to a nut is only one way to approximate stud tension: lubrication, thread and nut-face condition change the result (H.3). The same values are on the USC units page.

Stud Diameter D in. Threads per in. N 1/in. Studs with Sy = 720 MPa
Bolt Stress Equal to 360 MPa
Tension F kN Torque f = 0.07 N-m Torque f = 0.13 N-m
0.500 13 33 48 80
0.625 11 53 92 155
0.750 10 78 160 270
0.875 9 107 253 429
1.000 8 141 376 639
1.125 8 184 540 925
1.250 8 232 745 1285
1.375 8 286 996 1727
1.500 8 346 1297 2261
1.625 8 41 2 1653 2894
1.750 8 484 2069 3636
1.875 8 561 2549 4493
2.000 8 644 3097 5476
2.250 8 826 4418 7851
2.500 8 1032 6068 10,828
2.625 8 - - -
2.750 8 - - -
3.000 8 - - -
3.250 8 - - -
3.750 8 - - -
3.875 8 - - -
4.000 8 - - -

What does ASTM A453 Grade 660 Class D require?

ASTM A453 Grade 660 Class D is solution treated at 1650 ± 25 °F [900 ± 14 °C] for 2 h min or 1800 ± 25 °F [980 ± 14 °C] for 1 h min and liquid quenched, then aged at 1325 ± 25 °F [720 ± 14 °C] for 16 h and air cooled, with a second age at 1200 ± 25 °F [650 ± 14 °C] for 16 h if needed to reach the properties (A453/A453M-17 Table 4). Table 5 requires up to 2½ in. [63.5 mm]: 130 ksi [895 MPa] tensile and 105 ksi [725 MPa] yield; over 2½ in. [63.5 mm]: 120 ksi [825 MPa] tensile and 95 ksi [655 MPa] yield; 15 % elongation, 18 % reduction of area and 248 to 321 HB (24 to 35 HRC) in both size ranges.

Class D does not require a stress-rupture test and is stamped NR in addition to the other required markings (8.2.1, 9.1). Each bolting component carries the grade symbol and class (660 D) and the thread type: M1 or M2 for machined threads, R1 or R2 for rolled threads, formed after (1) or before (2) the precipitation heat treatment (6.1.1, 9.1). The 35 HRC maximum matches the ISO 15156-3 (NACE MR0175) limit for UNS S66286. API 20F covers Grade 660 Class D for BSL-2 and BSL-3 bolting, and API 6A (21st edition) 8.2.3.6 cautions against Grade 660D on pressure-containing connectors in salt-air offshore or coastal service, or where equipment is washed with raw seawater. See the ASTM A453 660D (Class D) specification, ASTM A453 Grade 660 chemical composition and mechanical properties.

Same table in US customary units: API 6A Bolting Torque for Flanges (USC Units). Stud forms: ASTM A453 Grade 660 Class D API 6A Full Thread Stud Bolt, ASTM A453 Grade 660 Class D API 6A Tap End Stud Bolt.

Source: ASTM A453/A453M-17; API 6A 21st edition; API 20F; ISO 15156-3. Last reviewed .

Specifications
  • ASTM A453
  • ASTM A638
  • EN 10269
  • EN 10083-3
  • ISO 3506-5
  • DIN 267
Surface Treatments
  • Xylan 1070 / 1014 / 1400 / 1424
  • Xylar 2 / 101
  • SermaGard 1105 / 1280
  • Dacromet 320 / 500
  • TakeCoat 1000 Ceramic
  • Magnigard
  • MolyKote
Certifications
  • ISO 9001 - 2015 Certified
  • PED 2014/68/EC
  • NACE MR0175/ISO 15156-2
  • NORSOK M-650
  • DFAR
  • MERKBLATT AD 2000 W2/W7/W10