A453 Grade 660 rods are often used for valves and pump stems. Due to high resistance to creep and stress, Grade 660 Rods are preferred over phosphor bronze and stainless steel 410. A453 Gr.660 rods can be offered from stock with both 3.1 & 3.2 certification. Grade 660 Rods stock is also used for machined components and hence bright finish with h9 tolerance is also available exstock.
Which ASTM A453 Grade 660 class do you need?
ASTM A453/A453M-17 sets four Grade 660 (UNS S66286) classes by heat treatment (Table 4) and strength (Table 5):
ASTM A453 Grade 660 Class C Rods: 1800 °F [980 °C] solution treatment with oil quench, double aged at 1425 °F [775 °C] and 1200 °F [650 °C]; 130 ksi [895 MPa] tensile, 85 ksi [585 MPa] yield, 24 to 37 HRC.
ASTM A453 Grade 660 Class D Rods: 105 ksi [725 MPa] yield up to 2½ in. [63.5 mm], 95 ksi [655 MPa] above; 24 to 35 HRC; no stress-rupture test, stamped NR. Covered by API 20F for BSL-2 and BSL-3 bolting.
Source: ASTM A453/A453M-17; API 20F. Last reviewed .